CHROMVEST
Phosphate investment for the casting in nickel-chrome or chrome-cobalt alloy. The product has to be mixed, according to the desired expansion, with "ESPANSOL" either pure or diluted with distilled water.
Technical features:
Mixing ratio:
15-17 ml. of liquid x 100 g. of powder
Working time:
3/4 min
Setting time:
7/8 min
Setting expansion:
0,5%
Thermic expansion:
1,1%
Maximal temperature of the investment:
1500°C
-Safety data sheet Chromvest (.pdf)